Grades | Stainless Steels | SA-1008 BHS Grade 44[300]

AMS SA-1008 BHS Grade 44[300] ( Ferrite )

PDF | Word | Print

SA-1008 BHS Grade 44[300] Application:Specification for Steel, Sheet, Cold-Rolled, Carbon, Structural, High-Strength Low-Alloy and High-Strength Low-Alloy With Improved Formability

Chemical composition(mass fraction)(wt.%) of the SA-1008 BHS Grade 44[300]
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Mn - 1.00
Si - 1.00
P - 0.04
S - 0.03
Cr 18.00 23.00
Ni - 0.50
Mo - -
Cu 0.90 1.25

Mechanical properties of grade SA-1008 BHS Grade 44[300]

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
118 (≥) 876 (≥) 24 32 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade SA-1008 BHS Grade 44[300]

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
714 (≥) 357 (≥) 33 12 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
388 445 522 - - -

SA-1008 BHS Grade 44[300] Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED